New arrival hot sale woodworking glue 2021 WPPS1 Two-component puzzle glue water-based polymer isocyanate adhesive
WPPS1 Series | |
Commodity: | WPPS1 Two-component puzzle glue water-based polymer isocyanate adhesive
|
Name: | Two-component Puzzle Glue |
The Amount Of Cloth Glue:: | 180-250 G/m2 |
Pressurizing Pressure:: | 7.0-10.0 Kg/cm² For Low-density Materials, 9.0-12.0 Kg/cm² For Medium-density Materials, 12.0-17.0 Kg/cm² For High-density Materials |
Storage:: | 9 Months, Sealed And Packaged At 25°C. Store Sealed In A Clean, Cool And Dry Place With A Temperature Between 5-30°C. |
Characteristic:: | Volatile Solvent Adhesives |
Classification: | Wood Glue |
Application: | Construction, Woodworking, Footwear & Leather, Fiber & Garment, Packing, Construction, Fiber & Garment, Footwear & Leather |
List of model parameters
Product name | PH | Solid content/% | Viscosity/25℃ | Characteristics and applicability |
PG1973-8/C15 | 7±1 | 50±2 | 11000±2000 | It is suitable for the integrated panel of hard maple, ash, oak, oak and other medium-hard materials. The JAS standard boiling water immersion peel test has a good performance, and the European D4 waterproof level meets the F☆☆☆☆ standard. |
PG1963/1 /C15 | 7±1 | 48±2 | 11000±2000 | It is suitable for the integrated panel of hard maple, ash, oak, oak and other medium-hard materials. The JAS standard boiling water immersion peel test has a good performance, and the European D4 waterproof level meets the F☆☆☆☆ standard. |
PG355/C15 | 7±1 | 50±2 | 11000±2000 | It is suitable for the integrated panel of hard maple, ash, oak, oak and other medium-hard materials. The JAS standard boiling water immersion peel test has a good performance, and the European D4 waterproof level meets the F☆☆☆☆ standard. |
PG368/C15 | 7±1 | 43±2 | 11000±2000 | It is suitable for the integrated panel of hard maple, ash, oak, oak and other medium-hard materials. The JAS standard boiling water immersion peel test has a good performance, and the European D4 waterproof level meets the F☆☆☆☆ standard. |
PG1268/C15 | 7±1 | 50±2 | 11000±2000 | It is suitable for the integrated panel of hard maple, ash, oak, oak and other medium-hard materials. The JAS standard boiling water immersion peel test has a good performance, and the European D4 waterproof level meets the F☆☆☆☆ standard. |
PG126/C15 | 7±1 | 50±2 | 11000±2000 | It is suitable for the integrated jigsaw of Southwest birch, rubber wood, miscellaneous wood, catalpa wood, elm and other medium-to-hard materials. JAS standard room temperature water and boiling water immersion peel tests have good performance. The European D4 waterproof level meets F☆ ☆☆☆Standard. |
PG134/AX | 7±1 | 50±2 | 11000±2000 | It is suitable for the integrated jigsaw of Southwest birch, rubber wood, miscellaneous wood, catalpa wood, elm and other medium-to-hard materials. JAS standard room temperature water and boiling water immersion peel tests have good performance. The European D4 waterproof level meets F☆ ☆☆☆Standard. |
Application note
1. The moisture content of wood is 8-14%, and the high moisture content needs to double the pressing time. Too high wood moisture content will cause cracks due to shrinkage during the drying process.
2. In order to obtain a significant effect, the surface of the wood must be planed. In order to obtain better gluing strength, gluing should be implemented within 24 hours after wood planing. For wood with oily or resin content, gluing should be implemented within 4 hours after wood planing.
3. After pressing, check whether the glue is evenly squeezed out of the glue line to determine whether the amount of glue is appropriate. The higher the density of the wood, the greater the environmental humidity, and the lower the environmental temperature, the longer the closing time.
4. Please complete the environment temperature above 25℃ within 5 minutes. The longer the aging time, the higher the viscosity of the adhesive layer and the lower the permeability. The aging time after cloth glue usually varies with the amount of cloth glue and the temperature and humidity of the operating environment. The shorter the aging time, the faster the pressure is applied, and the better the bonding strength can be ensured.
5. After the pressure is relieved, the board should be kept for at least 4 hours after the indoor temperature is above 25℃ before entering the next process. After 7 days of curing, it will reach the super good bonding strength.
6. When the feeding speed is more than 25m/min, please increase the temperature of the rubber box to 210°C.
Operation and use: Protective gloves and goggles should be worn for each use.
Cleaning: Use warm water to wash the skin and the glue on the equipment. The product must be cleaned before curing.
Health, Environmental Protection and Safety: Burns-Do not try to remove the glue that has cooled down on the skin. Seek medical advice.
Hot fumes-do not breathe. Use in a well-ventilated area.
Fire risk-use at the recommended operating temperature.